Overall, the difficulties in processing titanium alloys can be attributed to the following four core reasons, which work together to result in short tool life, low processing efficiency, and high costs:

Core Difficulty 1: Poor Thermal Conductivity - 'Heat cannot dissipate, causing the tool to burn out'
Problem Description: The thermal conductivity of titanium alloys is very low, approximately only 1/5 that of steel and 1/16 that of aluminum. This means that the large amount of heat generated during the cutting process cannot be quickly dissipated through the chips or the workpiece.
Direct consequence: Up to 80% of the cutting heat accumulates on the narrow cutting edge of the tool, causing extremely high local temperatures at the tip (which can easily exceed 1000°C even at lower cutting speeds). High temperatures rapidly soften the tool material, leading to rapid wear and chipping. This is the main reason limiting the increase in cutting speed.
Core Challenge 2: High Chemical Reactivity and Affinity - 'Tool Adhesion, Tearing Off Tool Material'
Problem Description: Titanium is highly reactive chemically at high temperatures and easily reacts with most tool materials (especially the cobalt in cemented carbide), resulting in 'affinity.'
Direct Consequence: This leads to severe 'built-up edge wear' and 'diffusion wear.' Molten titanium sticks to the tool surface like 'glue,' and under the brushing of chips, it tears off the tool material bit by bit. This limits the increase of cutting speed and causes abnormal tool failure.
Core Challenge 3: High strength while maintaining high-temperature strength - "Hard and tough, with enormous cutting forces"
Problem Description: Titanium alloys have a very high strength-to-weight ratio. More importantly, they retain very high strength and hardness at elevated temperatures (i.e., they have good "high-temperature strength" or "thermal strength"). When machining ordinary steel, the heat generated in the cutting zone softens the material, making cutting easier; however, titanium alloys remain "sturdy" even at high temperatures.
Direct Consequence: Very high cutting forces are required, which demands that the cutting tool itself must have extremely high strength and toughness, otherwise chipping or breakage can occur. The enormous cutting forces also place high demands on the machine tool's power and the rigidity of the process system.
Core Difficulty 4: Low Elastic Modulus - 'Tool deflection, vibration, difficult to ensure machining accuracy'
Problem Description: Titanium alloys have a relatively low elastic modulus, meaning they are 'softer' and less rigid.
Direct Consequences:Tool Deflection: Under cutting forces, the workpiece (especially thin-walled parts) is prone to elastic deformation, and it springs back after machining, causing the actual cutting depth to be less than the set value, which affects machining accuracy and dimensional stability.Vibration and Chatter: They easily induce cutting vibrations, which not only affect surface quality but also subject the tool to alternating stress, leading to premature chipping.
Increased Flank Wear: The machined surface produces strong friction with the tool's flank due to elastic recovery, accelerating flank wear.